Properties
Composition…High concentrated waxy oil derivative | Solid content(%)…. 76 ± 2% |
Appearance..... White to light yellow flake | Ionic ……....Nonionic/Anionic |
pH(1%)…..…..6.5 ± 1 | Solubility…. Easily soluble in water |
Instruction:
Direct input method:Directly add the paste melting in 60℃ during the heating process or after 1-1.5 hours melting.
Cast paste method:After the starch melting in the 65℃ for 20 minutes, stop the steam and add Caoil-200 in the starch dispersion of tank.
※We recommend you add Caoil-200 in 60℃ for the stability.
Application
For synthetic fiber and its blends, apply in 8~10% of starch, but when you apply in AFTERWAXING, dosage 2 ~ 3% is enough.
The dosage is 6~7% of starch in high class fabric.
Packing and storage
Net in 20 kg in water proof PP bag. Storage time 6 months,We suggest keep goods in cool and dry place.